Time and temperature reduction of the sealing process of porous aluminium oxide films with organic additives

Authors

  • A. Bautista Centro Nacional de Investigaciones Metalúrgicas, CENIM (CSIC)
  • V. López Centro Nacional de Investigaciones Metalúrgicas, CENIM (CSIC)
  • E. Otero Centro Nacional de Investigaciones Metalúrgicas, CENIM (CSIC)
  • R. Lizarbe Centro Nacional de Investigaciones Metalúrgicas, CENIM (CSIC)
  • J. A. González Centro Nacional de Investigaciones Metalúrgicas, CENIM (CSIC)

DOI:

https://doi.org/10.3989/revmetalm.1998.v34.iExtra.708

Keywords:

Anodizing, New sealing methods, Sealing times reduction, Lowering sealing tempertures

Abstract


Different sealing processes of anode coatings in aluminium oxide have been industrially used for more than 30 years. In two of the preceeding decades a great effort was realized to reduce costs in the traditional hydrothermal sealing process in deionized boiling water (SHT), a very expensive process due to its endurance and high temperature on which it develops. New sealing procedures are proposed, on which by means of the use of organic additives, the time or the temperature of the SHT is essentially reduced.

Downloads

Download data is not yet available.

Downloads

Published

1998-05-30

How to Cite

Bautista, A., López, V., Otero, E., Lizarbe, R., & González, J. A. (1998). Time and temperature reduction of the sealing process of porous aluminium oxide films with organic additives. Revista De Metalurgia, 34(Extra), 57–61. https://doi.org/10.3989/revmetalm.1998.v34.iExtra.708

Issue

Section

Articles

Most read articles by the same author(s)

<< < 1 2 3 4 > >>