Micro/nanostructured coatings of light alloys by cold spray for surface protection and repair of high value-added components: State of the art

Authors

  • J. Bedoya Centre de Projecció Tèrmica (CTP). Universitat de Barcelona
  • N. Cinca Centre de Projecció Tèrmica (CTP). Universitat de Barcelona
  • J. M. Guilemany Centre de Projecció Tèrmica (CTP). Universitat de Barcelona

DOI:

https://doi.org/10.3989/revmetalm.1237

Keywords:

Cold Gas Spray (CGS), Light alloys, Weld overlay, Brazing, Coatings

Abstract


The Cold Gas Spray - CGS technique has greatly attracted the attention of the researchers in the last decade due to advantages compared to other conventional thermal spray processes. It presents outstanding characteristics such as high density coatings and absence of thermal degradation (oxidation or phase transformation). In addition, CGS is an efficient and green technology. This paper presents a bibliographic review related to micro/nanostructured aluminium-based coatings of by CGS on light alloy substrates. It provides an overview of the feasibility of using the Cold Gas Spray as a technique for the protection, recovery and repair of high value-added components, especially those made of light alloys (aluminium and magnesium base) which, by their low density and mechanical properties, are widely used in several industrial sectors such as transport, aerospace and power generation.

Downloads

Download data is not yet available.

References

[1] T. Sidhu, S. Prakash y R. Agrawal, Corros. Eng. Sci. Techn. 43 (2008) 335-342. http://dx.doi.org/10.1179/174327808X286446

[2] R.C. Souza, H. Voorwald y M. Cioffi, Surf. Coat. Tech. 203 (2008) 191-198. http://dx.doi.org/10.1016/j.surfcoat.2008.07.038

[3] J.M. Guilemany, J. Fernández, A.V. Benedetti y J. Delgado, Proc. International Thermal Spray Conference, ASM Thermal Spray Society, Dusseldorf, Germany, 2002, pp. 894-899.

[4] J. Fernández, M. Gaona y J.M. Guilemany, J. Therm. Spray Techn. 16 (2007) 220-228. http://dx.doi.org/10.1007/s11666-007-9034-7

[5] H. Herman, S. Sampath y R. McCune, Mater. Res. Bull. 25 (2000) 17-25.

[6] J.M. Guilemany, N. Cinca, J. Fernández y S. Sampath, J. Therm. Spray Techn. 17 (2008) 762-773. http://dx.doi.org/10.1007/s11666-008-9252-7

[7] A.E. Segall, A.N. Papyrin, J.C. Conway Jr. y D. Shapiro, JOM 50 (1998) 52-54. http://dx.doi.org/10.1007/s11837-998-0417-0

[8] E. Irissou, J.G. Legoux, A.N. Ryabinin, B. Jodoin y C. Moreau, J. Therm. Spray Techn. 17 (2008) 495-516. http://dx.doi.org/10.1007/s11666-008-9203-3

[9] H. Assadi, F. Gärtner, T. Stoltenhoff y H. Kreye, Acta Mater. 51 (2003) 4.379-4.394. http://dx.doi.org/10.1016/S1359-6454(03)00274-X

[10] A.N. Papyrin, V.F. Kosarev, S.V. Klinkow y A.P. Alkhimov, Proc. International Thermal Spray Conference, Dusseldorf, Germany, 2002, pp. 380-384.

[11] M. Hammerschidt y H. Kreye, Shock waves and high strain-rate phenomena in metals, Ed. M.A. Meyers, L.E. Murr, Plenum Press, New York, 1981, p. 961. http://dx.doi.org/10.1007/978-1-4613-3219-0_54

[12] T.H. Van Steenkiste, J.R. Smith y R.E. Teets, Surf. Coat. Tech. 154 (2002) 237-252. http://dx.doi.org/10.1016/S0257-8972(02)00018-X

[13] T.H. van Steenkiste, J.R. Smith y R.E. Teets, Surf. Coat. Tech. 111 (1999) 62-71. http://dx.doi.org/10.1016/S0257-8972(98)00709-9

[14] D.L. Gilmore, R.C. Dykhuizen, R.A. Neiser, T.J. Roemer y M.F. Smith, J. Therm. Spray Techn. 8 (1999) 576-582. http://dx.doi.org/10.1361/105996399770350278

[15] M. Villa, S. Dosta, J. Fernández y J. M. Guilemany, Rev. Metal. 48 (2012) 175-191. http://dx.doi.org/10.3989/revmetalm.1111

[16] R.C. Dykhuizen y M.F. Smith, J. Therm. Spray Techn. 7 (1998) 205-212. http://dx.doi.org/10.1361/105996398770350945

[17] C.J. Li y W.Y. Li, Surf. Coat. Tech. 167 (2003) 278-283. http://dx.doi.org/10.1016/S0257-8972(02)00919-2

[18] R. Kapoor y S. Nemat-Nasser, Mech. Mater. 27 (1998) 1-12. http://dx.doi.org/10.1016/S0167-6636(97)00036-7

[19] J.F. Molinari y M. Ortiz, Int. J. Impact. Eng. 27 (2002) 347-358. http://dx.doi.org/10.1016/S0734-743X(01)00055-0

[20] S. Dosta, C. Lorenzana, N. Cinca y J. M. Guilemany, Soldadura y Tecnologías de Unión 126 (2011) 13-14.

[21] D.S. Mehta, S.H. Masood y W.Q. Song, J. Mater. Process. Tech. 155 (2004) 1.526-1.531. [22] S. Das, JOM 55 (2003) 22-26. http://dx.doi.org/10.1007/s11837-003-0204-x

[23] M.G. Fontana,Corrosion Engineering, 3rd ed., McGraw-Hill International Editions, 1996, p. 42.

[24] J.E. Gray y B. Luan, J. Alloy. Compd. 336 (2002) 88-113. http://dx.doi.org/10.1016/S0925-8388(01)01899-0

[25] X. Cao, M. Jahazi, J.P Immarigeon y W. Wallace, J. Mater. Process. Tech. 171 (2006) 188. http://dx.doi.org/10.1016/j.jmatprotec.2005.06.068

[26] K.B Armstrong, Int. J. Adhes. Adhes. 3 (1983) 37-52. http://dx.doi.org/10.1016/0143-7496(83)90051-9

[27] W.Y. Li, C. Zhang, X. Guo, C.J. Li, H. Liao, y C. Coddet, Appl. Surf. Sci. 254 (2007) 517- 526. http://dx.doi.org/10.1016/j.apsusc.2007.06.026

[28] W.Y. Li, H. Liao, H.T. Wang, C.J. Li, G. Zhang, y C. Coddet, Appl. Surf. Sci. 253 (2006) 708- 713. http://dx.doi.org/10.1016/j.apsusc.2005.12.157

[29] D. Zhang, P. Shipway, y D. McCartney, J. Therm. Spray Techn. 14 (2005) 109-116. http://dx.doi.org/10.1361/10599630522666

[30] X.J. Ning, J.H. Jang, y H.J. Kim, Appl. Surf. Sci. 253 (2007) 7.449-7.455. http://dx.doi.org/10.1016/j.apsusc.2007.03.031

[31] A.O. Tokarev,Met. Sci. Heat Treat. 38 (1996) 136-139. http://dx.doi.org/10.1007/BF01401446

[32] F. Gil, C. Aparicio y D. Rodrígues, Aleaciones ligeras, Ed. Edicions UPC, Barcelona. Espa-a, 2001, p. 251.

[33] J. Wu, H. Fang, S. Yoon, H. Kim, y C. Lee, Scripta Mater. 54 (2006) 665-669. http://dx.doi.org/10.1016/j.scriptamat.2005.10.028

[34] L. Zhao, K. Bobzin, D. He, J. Zwick, F. Ernst y E. Lugscheider, Adv. Eng. Mater. 8 (2006) 264- 267. http://dx.doi.org/10.1002/adem.200500227

[35] W.Y. Li, C. Zhang, X.P. Guo, G. Zhang, H.L. Liao, y C. Coddet, Appl. Surf. Sci. (2007) 7.124-7.130.

[36] V.K Champagne, D.J Helfritch, M.D Trexler y B.M Gabriel, Modell. Simul. Mater. Sci. Eng. 18 (2010) 1-8. http://dx.doi.org/10.1088/0965-0393/18/6/065011

[37] R. Rofagha, R. Langer, A.M. El-Sherik, U. Erb, G. Palumbo y K.T. Aust, Scr. Metall. Mater. 25 (1991) 2.867-2.872. http://dx.doi.org/10.1016/0956-716X(91)90171-V

[38] R.B. Intrui y Z. Szklarska-Smialowska, Corrosion 48 (1992) 398-403. http://dx.doi.org/10.5006/1.3315951

[39] E. Sikora, X.J. Wei, y B.A. Shaw, Corrosion 60 (2004) 387-398. http://dx.doi.org/10.5006/1.3287748

[40] M.M. Sharma y C.W. Ziemian, J. Mater. Eng. Perform. 17 (2008) 870-878. http://dx.doi.org/10.1007/s11665-008-9215-7

[41] L. Liu, Y. Li y F. Wang, Electrochim. Acta. 54 (2008) 768-780. http://dx.doi.org/10.1016/j.electacta.2008.06.076

[42] L. Liu, Y. Li y F. Wang, Electrochim. Acta. 53 (2008) 2.453-2.462.

[43] J. Bedoya, S. Dosta, N. Cinca y J.M. Guilemany, XII Congr. Nac. de Materiales, Universidad de Alicante, CD-Rom ISBN978-84-695-3316-1, Sociedad Espa-ola de Materiales, Alicante, Espa-a, 2012.

[44] M.A. Haque y M.T.A. Saif, Thin Solid. Films 484 (2010) 364-368. http://dx.doi.org/10.1016/j.tsf.2005.02.036

[45] E.L. Dreizin, Prog. Energy Combust. Sci. 35 (2009) 141-167. http://dx.doi.org/10.1016/j.pecs.2008.09.001

[46] C. Goujon, P. Goeuriot, M. Chedru, J. Vicens, J.L. Chermant, F. Bernard, J.C. Niepce, P. Verdier, e Y. Laurent, Powder Technol. 105 (1999) 328-336. http://dx.doi.org/10.1016/S0032-5910(99)00155-2

[47] C. Junsheng, C. Hua, C. Hanbin, Y. Bin, F. Jianzhong, y Z. Jishan, J. Univ. Sci. Technol. B. 14 (2007) 523-528. http://dx.doi.org/10.1016/S1005-8850(07)60121-2

[48] C.C. Koch, Nanostruct. Mater. 9 (1997) 13- 22. http://dx.doi.org/10.1016/S0965-9773(97)00014-7

[49] E.J. Lavernia, B.Q. Han, y J.M. Schoenung, Mater. Sci. Eng. A. 493 (2008) 207-214. http://dx.doi.org/10.1016/j.msea.2007.06.099

[50] W.Y. Li, G. Zhang, C. Zhang, O. Elkedim, H. Liao, y C. Coddet, J. Therm. Spray Techn. 17 (2008) 316-322. http://dx.doi.org/10.1007/s11666-008-9182-4

[51] N.Cinca, E. Hurtado, I.G. Cano y J.M Guilemany, Rev. Metal. 47 (2011) 197- 204. http://dx.doi.org/10.3989/revmetalm.1028

[52] F. Zhou, D. Witkin, S.R. Nutt, y E.J. Lavernia, Mater. Sci. Eng. A. 375 (2004) 917-921. http://dx.doi.org/10.1016/j.msea.2003.10.235

[53] L. Ajdelsztajn, J. Schoenung, B. Jodoin, y G. Kim, Metall. Mater. Trans. A 36 (2005) 657- 666. http://dx.doi.org/10.1007/s11661-005-0182-4

[54] Y. Zhang, X. Wu, H. Cui, y J. Zhang, J. Therm. Spray Techn. 20 (2011) 1.125-1.132. http://dx.doi.org/10.1007/s11666-010-9600-2

[55] F. Wendl y K.D. Wupper, J. Mater. Process. Tech. 24 (1990) 355-364. http://dx.doi.org/10.1016/0924-0136(90)90196-2

[56] L. Zhao, K. Bobzin, F. Ernst, J. Zwick, J. Roesing, y E. Lugscheider, Adv. Eng. Mater. 8 (2006) 751-753. http://dx.doi.org/10.1002/adem.200600001

[57] K. Bobzin, L. Zhao, T. Schlaefer, y T. Warda, Front. Mech. Eng. Chin. 5 (2010) 256-260. http://dx.doi.org/10.1007/s11465-010-0095-9

[58] V. Luzin, K. Spencer, y M.X. Zhang, Acta Mater. 59 (2011) 1.259-1.270. http://dx.doi.org/10.1016/j.actamat.2010.10.058

[59] J. Villafuerte y D. Wright, ASM Thermal Spray Society., 5 (2010) 13-15

[60] P.F. Leyman y V.K. Champagne, U.S. Army Research Laboratory, ARL Report Nº ARLTR- 4922, 2009, pp. 1-22.

[61] V.K. Champagne, P.F. Leyman, y D.J. Helfritch, U.S. Army Research Laboratory, ARL Report Nº ARL-TR-4438, 2008, pp. 1-26.

[62] J.C. Lee, H.J. Kang, W.S. Chu, y S.H. Ahn, CIRP Ann. Manuf. Techn. 56 (2007) 577-580. http://dx.doi.org/10.1016/j.cirp.2007.05.138

[63] J. Miguel, S. Vizcaíno, S. Dosta, N. Cinca, C. Lorenzana y J.M Guilemany, Rev. Metal. 47 (2011) 390-401. http://dx.doi.org/10.3989/revmetalm.1045

[64] S. Dosta, N. Cinca y J.M. Guilemany, International Thermal Spray Conference ITSC 2012, ASM Thermal Spray Society, Houston, EE.UU., 2012.

Downloads

Published

2013-06-30

How to Cite

Bedoya, J., Cinca, N., & Guilemany, J. M. (2013). Micro/nanostructured coatings of light alloys by cold spray for surface protection and repair of high value-added components: State of the art. Revista De Metalurgia, 49(3), 223–236. https://doi.org/10.3989/revmetalm.1237

Issue

Section

Reviews

Most read articles by the same author(s)

1 2 > >>