Protection against salt water of the AA5083 alloy by treatments based on lanthanides salts
DOI:
https://doi.org/10.3989/revmetalm.1998.v34.iExtra.706Keywords:
Environmental friendly surface pretreatments, Aluminium alloys, Lanthanide elementsAbstract
AA5083 sheet samples have been pre-treated by full immersion in aqueous solutions of different lanthanide trichlorides salts, namely CeCl3, LaCl3 and SmCl3 The inhibition against uniform and pitting corrosión, in 3.5 % NaCl solutions, provided by such surface treatments has been estimated using electrochemical techniques. Protection against pitting has been quantified in terms of the percentage of increase observed for the pitting nucleation resistance. Among all the pretreatments tested, optimum performances have been observed for those carried out in 500 ppm CeCl3 aqueous solutions for fifteen days. However, acceptable protection degrees are observed even after 48 h in this solution.
Downloads
Downloads
Published
How to Cite
Issue
Section
License
Copyright (c) 1998 Consejo Superior de Investigaciones Científicas (CSIC)

This work is licensed under a Creative Commons Attribution 4.0 International License.
© CSIC. Manuscripts published in both the printed and online versions of this Journal are the property of Consejo Superior de Investigaciones Científicas, and quoting this source is a requirement for any partial or full reproduction.
All contents of this electronic edition, except where otherwise noted, are distributed under a “Creative Commons Attribution 4.0 International” (CC BY 4.0) License. You may read the basic information and the legal text of the license. The indication of the CC BY 4.0 License must be expressly stated in this way when necessary.
Self-archiving in repositories, personal webpages or similar, of any version other than the published by the Editor, is not allowed.