Time and temperature reduction of the sealing process of porous aluminium oxide films with organic additives
DOI:
https://doi.org/10.3989/revmetalm.1998.v34.iExtra.708Keywords:
Anodizing, New sealing methods, Sealing times reduction, Lowering sealing temperturesAbstract
Different sealing processes of anode coatings in aluminium oxide have been industrially used for more than 30 years. In two of the preceeding decades a great effort was realized to reduce costs in the traditional hydrothermal sealing process in deionized boiling water (SHT), a very expensive process due to its endurance and high temperature on which it develops. New sealing procedures are proposed, on which by means of the use of organic additives, the time or the temperature of the SHT is essentially reduced.
Downloads
Downloads
Published
How to Cite
Issue
Section
License
Copyright (c) 1998 Consejo Superior de Investigaciones Científicas (CSIC)

This work is licensed under a Creative Commons Attribution 4.0 International License.
© CSIC. Manuscripts published in both the printed and online versions of this Journal are the property of Consejo Superior de Investigaciones Científicas, and quoting this source is a requirement for any partial or full reproduction.
All contents of this electronic edition, except where otherwise noted, are distributed under a “Creative Commons Attribution 4.0 International” (CC BY 4.0) License. You may read the basic information and the legal text of the license. The indication of the CC BY 4.0 License must be expressly stated in this way when necessary.
Self-archiving in repositories, personal webpages or similar, of any version other than the published by the Editor, is not allowed.